(Bundle Sale) TPU Filament,0.5kg (MOQ:10 Rolls,Mixable)

$21.99 $16.99 Save 23%
Shipping calculated at checkout.
Pros
Affordable: Bundle sale, MOQ 10 rolls, mixable, from $21.99/spool.
Tough & Resilient: Durable, breaks - resistant, withstands water, heat, and oil.
Clear Guidelines: Specific printing settings ensure smooth 3D printing process.
SHIP TO: CA (TO CA ONLY)
Color: Gray
SHIP TO
Color: Gray

Feature:

  • Having higher toughnessthan PLA.
  • Having higher hardness than PLA.
  • The impact strength is more than 30 times that of standard PLA.
  • Elongationat break is more than 50 times that of standard PLA.
  • Adhesive force is stronger than that of PLA.

Specifications:

  • Filament Diameter: 1.75 mm
  • Tolerance: ±0.03 mm
  • Printing Temperature: 230°C-250°C
  • Heated Bed Temperature: 70-85°C
  • Printing Speed:30-80mm/s

PETG Review by Michele Dicati

ERYONE - Tutti i Test del filamento PLA + e PETG


 

FAQ

1.Q: Why my filament tangles? How can I solve it?

A: The tangle of filament isn’t caused by the disordered or the imperfect winding. According to the production technology of filament, the filament winds back and forth (from left to right and then from right to left). Normally, there is no overline tangle. A common cause of tangle is that the filament end is not fixed to the holes of spool. Overline tangle or the changed winding direction make filament tangle. So customers need to fix the filament end to the proper holes of the spool.

  1. Q: Is PETG degradable?

A: The natural degradation process of PETG raw materials is very long, and PETG is a non-degradable material. PETG is a thermoplastic material, which can be used for secondary plastic recycling. PETG is also an environmentally friendly material.

3.Q: The nozzle is clogged by PETG, and how can I solve it?

  A:  Inconstant filament diameter, the lower nozzle temperature and frequent replacement with different kinds of filaments will lead to this problem. So, before you get started, clean the nozzle and turn up the temperature to a proper value.

4.Q: My prints have web-like strings (stringing) issues. How can I troubleshoot it?

  A: Too high temperature makes the PETG filament melt and flow so fast. Please turn the temperature down to a proper value.  

      The retracting parameters are improper, so adjust the retracting length and speed.  

5.Q: There are too much melted filament around the nozzle. What should I do?

  A: This problem can be attributed to over-high temperature, low printing speed, and in the slice software, the nozzle diameter doesn’t match with the extrusion output.

6.Q: The PETG filament was perfect when I opened the package. After several times of intermittent printing, my PETG filament snaps by accident during printing. Why?

A: Normally, the PETG filament in the printing process will not snap by themselves. However, after being affected by moisture, the degradable material PETG will be more brittle and easier to break, so you should pay attention to dampproof.

7.Q: The surface of my print isn’t very smooth, and the extruded filament has inconstant diameters. Why?

  A: The printing temperature is too high or too low. The temperature doesn’t match well with the printing speed. You need to adjust the printing speed or temperature.

8.Q: Why my PETG-printed objects don't stick to the heated bed? How do I solve?

A: The distance between the nozzle and the bed is too far. Make sure your heated bed is levelled and it’s clean. Then judge if the printing temperature and heated bed temperature are too low, and our customers should adjust them to correct ranges.

High Speed TPU Printing

ERYONE TPU filament 1.75mm is designed for hyper speed printing, 30-300mm/s up to 5 times faster than regular TPU filament, providing a smooth and efficient 3D printing experience.

Improve the performance of TPU Filament

Make it easy to print, faster than previous TPU, excellent adhesion. Clog-Free, Bubble-Free, Low-Warp, Low-String.

Standard TPU Material

is a polymer material between rubber and plastic. It has excellent high tension, high tensile strength, toughness and aging resistance. It is a mature environmental protection material. TPU consumables are added on the basis of raw materials. The material is environmentally friendly.

Standard TPU Technical Specification

Print Temperature:190 - 220℃, Diameter:1.75mm (Tolerance:+/-0.05mm). Shore hardness 95A, Net weight 1kg2.2lbs), We recommend hardened steel nozzle 0.5mm.

FAQs

Can I use TPU on Bowden Extruder printer?

Yes. The material itself is soft and does not bear any force. It is recommended to use the direct drive extruder to get a good printing experience. The remote extruder can only print normally after modification.

Does the hot bed temperature need to be set?

No, you don't have to. You can print objects normally when the heated bed is at room temperature.

Why my filament tangles? How can I solve it?

The tangle of filament isn’t caused by the disordered or the imperfect winding. According to the production technology of filament, the filament winds back and forth (from left to right and then from right to left). Normally, there is no overline tangle. A common cause of tangle is that the filament end is not fixed to the holes of spool. Overline tangle or the changed winding direction make filament tangle. So customers need to fix the filament end to the proper holes of the spool.

The nozzle is clogged by TPU, and how can I solve it?

Inconstant filament diameter, the lower nozzle temperature and frequent replacement with different kinds of filaments will lead to this problem. So, before you get started, clean the nozzle and turn up the temperature to a proper value.